Boyanın iyice sertleşmesine izin verin, fazla boyayı alın, zımparalayın, pasta uygulayın ve cilalayın. Kusurun ağır olduğu durumlarda, yüzeyin zımparalanması ve yeniden boyanması gerekli olabilir.
NOT: Metalik renklerde kararma olacağı için yeniden boyanması gerekmektedir.
Description
Well defined local thickening of the paint film in the form of a wavy line or shallow, rounded ridges, normally confined to sharply sloping or vertical surfaces.
Cause
Slumping of the paint due to:
Excess thickness of application, air pressure too low, fan width too narrow, spray gun too close to the surface or moving too slowly.
Use of poor quality or incorrect thinner.
Incorrect viscosity of the paint.
Air of surface temperature too low.
Contamination of the underlying surface.
Prevention
Use the correct spraying technique and spray gun settings.
Use only recommended thinner.
Ensure that the paint is mixed to the correct viscosity.
Always spray within the recommended temperatures.
Ensure that the surface is scrupulously clean.
Rectification
Allow the paint to harden thoroughly, rub down excess paint, flat, compound and polish. In severe cases it may be necessary to rub down and repaint the surface.
NOTE: Due to separation of the metal flakes, metallic paints will normally require repainting.
Bu site, size en iyi deneyimi sunmak ve çerez politikamıza uygun olarak sizinle ilgili bilgi toplamak amacıyla çerezleri kullanmaktadır. Web sitemizi kullanmaya devam ederseniz, çerez ayarlarınızı değiştirmediğiniz sürece ppgrefinish.com web sitesinde çerezleri, çerez politikamızda açıklandığı şekilde almayı kabul ettiğinizi varsayacağız.